(Especially those with mill brands)
| Company | Location | Total Capy tpd |
Capacity, % | |
|---|---|---|---|---|
| Alk. | Alk. Free-sheet | |||
| Appleton | Newton Falls, NY | 350 | 100 | 100 |
| Badger | Peshtigo, WI | 225 | 100 | 100 |
| Boise Cascade | Internat Falls, MN | 1450 | 85 | 85 |
| Boise Cascade | Jackson, AL | 280 | 100 | 100 |
| Boise Cascade | St. Helens, OR | 700 | 87 | 87 |
| Boise Cascade | Wallula, WA | 590 | 100 | 100 |
| Byron Weston | Dalton, MA | 70 | ||
| Champion | Canton, NC | 709 | 100 | 100 |
| Champion | Cantonment, FL | 1100 | 0 | 0 |
| Champion | Courtland, AL | 2785 | 0 | 0 |
| Champion | Hamilton, OH | 400 | 33 | 33 |
| Champion | Quennesec, MI | 800 | 100 | 100 |
| Champion | Sartell, MN | 850 | 0 | 0 |
| Consolidated | Wisc. Rapids, WI | 1300 | 100 | 100 |
| Crane | Dalton, MA | 30 | ||
| Crane | Dalton, MA | 30 | ||
| Crane | Dalton, MA | 60 | ||
| Crown Vantage | Adams, MA | 45 | 50 | 50 |
| Crown Vantage | Gorham, NH | 445 | 75 | 75 |
| Crown Vantage | Newark, DE | 22 | 25 | 25 |
| Crown Vantage | Parchment, MI | 200 | 100 | 100 |
| Crown Vantage | St. Francisville, LA | 1000 | 0 | 0 |
| Crown Vantage | Ypsilanti, MI | 36 | 50 | 50 |
| Custom Papers Gp | Hughesville, NJ | 38 | ||
| Custom Papers Gp | Warren Glen, NJ | 75 | ||
| Eastern | Brewer, ME | 250 | 100 | 100 |
| Eastern | Lincoln, ME | 200 | 0 | 0 |
| Eddy | Port Huron, MI | 270 | 80 | 80 |
| Esleeck | Turners Falls, MA | 25 | ||
| Finch Pruyn | Glens Falls, NY | 675 | 100 | 100 |
| Fletcher | Alpena, MI | 85 | 100 | 100 |
| Fox River | Housatonic, MA | 50 | ||
| Fox River | Appleton, WI | 100 | 100 | 100 |
| Fox River | Ripon, CA | 95 | ||
| Fox River | Urbana, OH | 100 | ||
| Fox River | Vicksburg, MI | 125 | ||
| Fraser | Madawaska, ME | 600 | 42 | 42 |
| Fraser | Park Falls, WI | 375 | 100 | 100 |
| Fraser | W. Carrollton, OH | 310 | 100 | 100 |
| French | Niles, MI | 55 | 75 | 75 |
| Georgia-Pacific | Ashdown, AR | 2300 | 100 | 100 |
| Georgia-Pacific | Crossett, AR | 565 | 100 | 100 |
| Georgia-Pacific | Kalamazoo, MI | 400 | 0 | 0 |
| Georgia-Pacific | Nekoosa, WI | 600 | 100 | 100 |
| Georgia-Pacific | Port Edwards, WI | 450 | 100 | 100 |
| Georgia-Pacific | Woodland, ME | 340 | 0 | 0 |
| Georgia-Pacific | Zachary, LA | 1570 | 100 | 100 |
| Gilbert Paper | Menasha, WI | 120 | 5 | 5 |
| Glatfelter | Neenah, WI | 450 | 100 | 100 |
| Glatfelter | Pisgah Forest, NC | 300 | 100 | 100 |
| Glatfelter | Spring Grove, PA | 815 | 100 | 100 |
| Grays Harbor | Hoquiam, WA | 400 | 100 | 100 |
| Hennepin | Little Falls, MN | 100 | 20 | 20 |
| Internat'l Paper | Selma, AL | 1640 | 100 | 100 |
| Internat'l Paper | Erie, PA | 565 | 100 | 100 |
| Internat'l Paper | Georgetown, SC | 780 | ||
| Internat'l Paper | Hamilton, OH | 130 | 60 | 60 |
| Internat'l Paper | Jay, ME | 1500 | ||
| Internat'l Paper | Lock Haven, PA | 650 | 100 | 100 |
| Internat'l Paper | Moss Point, MS | 830 | ||
| Internat'l Paper | Ticonderoga, NY | 850 | 100 | 100 |
| Internat'l Paper | Bastrop, LA | 650 | ||
| Internat'l Paper | Mobile AL | 1170 | 100 | 100 |
| James River | Camas, WA | 1490 | 55 | 55 |
| James River | Clatskanie, OR | 300 | 100 | 100 |
| Kerwin | Appleton, WI | 145 | ||
| Kimberly-Clark | East Ryegate, VT | 75 | 10 | 10 |
| Kimberly-Clark | Munising, MI | 98 | 0 | 0 |
| Mead | Chillicothe, OH | 248 | ||
| Mead | Chillicothe, OH | 400 | 100 | 100 |
| Mead | Escanaba, MI | 1550 | 100 | 100 |
| Merrimac | Lawrence, MA | 104 | ||
| Mohawk | Cohoes, NY | 120 | 100 | 100 |
| Mohawk | Waterford, NY | 110 | 100 | 100 |
| Monadnock | Bennington, NH | 70 | ||
| Neenah | Neenah, WI | 125 | ||
| Neenah | Stevens Pt, WI | 220 | ||
| Nicolaus Paper | Lockport, LA | 50 | ||
| Parsons | Holyoke, MA | 35 | 100 | 100 |
| Potlatch | Brainerd, MN | 395 | 100 | 100 |
| Potlatch | Cloquet, MN | 540 | 100 | 100 |
| Repap Wisconsin | Kimberly, WI | 1400 | 100 | 100 |
| Schoeller Tech'l | Pulaski, NY | 100 | ||
| Seaman Paper | Otter River, MA | 75 | ||
| Simpson | Anderson, CA | 250 | 100 | 100 |
| Simpson | Gilman, VT | 200 | ||
| Simpson | Pomona, CA | 180 | 100 | 100 |
| Simpson | Vicksburg, MI | 260 | 100 | 100 |
| Simpson Pasadena | Pasadena, TX | 450 | 100 | 100 |
| Sorg | Middletown, OH | 85 | ||
| Southworth | W Springfield, MA | 25 | ||
| Strathmore | Millers Falls, MA | |||
| Strathmore | Woronoco, MA | 100 | 100 | |
| Union Camp | Eastover, SC | 1550 | 100 | 100 |
| Union Camp | Franklin, VA | 1900 | 80 | 80 |
| Warren | Hinkley/ Skowhegan, ME | 1800 | 100 | 100 |
| Warren | Mobile, AL | 840 | ||
| Warren | Muskegon, MI | 700 | ||
| Warren | Westbrook, ME | 200 | 100 | 100 |
| Wausau | Brokaw, WI | 480 | ||
| Wausau | Groveton, NH | 300 | 100 | 100 |
| Westvaco | Luke, MD | 1249 | ||
| Westvaco | Tyrone, PA | 200 | ||
| Westvaco | Wickliffe, KY | 600 | 100 | 100 |
| Weyerhaeuser | Longview, WA | 410 | 100 | 100 |
| Weyerhaeuser | Plymouth, NC | 1000 | 100 | 100 |
| Weyerhaeuser | Rothschild, WI | 350 | 100 | 100 |
| Whiting | Menasha, WI | 28 | 100 | 100 |
| Willamette | Bennettsville, SC | 700 | 100 | 100 |
| Willamette | Hawesville, KY | 550 | 100 | 100 |
| Willamette | Johnsonburg, PA | 1000 | 100 | 100 |
| Willamette | Kingsport, TN | 630 | ||