JAIC 1980, Volume 19, Number 2, Article 2 (pp. 69 to 74)
JAIC online
Journal of the American Institute for Conservation
JAIC 1980, Volume 19, Number 2, Article 2 (pp. 69 to 74)

THE RETENTION OF ORGANIC SOLVENTS IN PAPER

J. S. Arney, & L. B. Pollack


ABSTRACT—The retention of organic solvents in solvent-treated papers has been explored using gas chromatography. Results suggest that moisture in the atmosphere will displace retained solvents completely in a few hours under an ordinary environment. A related study of the sorption of thymol vapors by paper indicates that thymol also is not retained permanently in paper.

Article Sections:

1. INTRODUCTION
2. SOLVENT-CELLULOSE COMPLEXES
3. RESULTS AND DISCUSSION
4. CONCLUSIONS
5. EXPERIMENTAL
a: References
Entire Article

Copyright © 1980 American Institute of Historic and Artistic Works