COLORS AND OTHER MATERIALS OF HISTORIC WALLPAPER

Catherine Lynn


ABSTRACT—Published eighteenth- and nineteenth-century instructions for the making of wallpaper are examined, with particular attention given to the specific pigments recommended and their application.