JAIC 1981, Volume 20, Number 2, Article 9 (pp. 111 to 115)
JAIC online
Journal of the American Institute for Conservation
JAIC 1981, Volume 20, Number 2, Article 9 (pp. 111 to 115)

THE IN SITU TREATMENT OF THE WALLPAPER IN THE STUDY OF THE LONGFELLOW NATIONAL HISTORIC SITE

Thomas K. McClintock


ABSTRACT—The conservation of a room with the wallpaper painted one color is discussed in the context of a continuing project at a historic house. The treatment problems of such a wallpaper are contrasted with those of patterned wallpapers. The wallpaper was surface cleaned, mended, readhered to the wall at areas of detachment, and losses were filled and inpainted. The advantages and disadvantages of several treatment procedures and materials are discussed.

Article Sections:

1. INTRODUCTION
2. DESCRIPTION
3. CONDITION
4. TREATMENT
5. SUMMARY
a: References
Entire Article

Copyright © 1981 American Institute of Historic and Artistic Works