CONSOLIDATION OF DETERIORATED WOOD WITH SOLUBLE RESINS

Y. Wang, & A.P. Schniewind



4 OBJECTIVE

THE PURPOSE of this study was to determine the influence of type of soluble thermoplastic resin, type of solvent, resin concentration and drying rate of solvent on improvements in strengths and stiffness when resin solutions are impregnated into bacterically deteriorated wood.