JAIC 1986, Volume 25, Number 2, Article 3 (pp. 83 to 92)
JAIC online
Journal of the American Institute for Conservation
JAIC 1986, Volume 25, Number 2, Article 3 (pp. 83 to 92)

ON THE REVERSIBILITY OF TREATMENTS WITH ACRYLIC/SILICONE RESIN MIXTURES

A.E. Charola, A. Tucci, & R.J. Koestler


ABSTRACT—The reversibility of a consolidation treatment on limestone, using an acrylic/silicone mixture, is tested on aged and unaged specimens. Extracted residues are tested by infrared analysis and scanning electron microscope examination. Irreversibility of the treatment is found to be confined to the exposed surface of the stone.

Article Sections:

1. INTRODUCTION
2. EXPERIMENTAL
3. RESULTS AND DISCUSSION
4. CONCLUSIONS
a: Materials , References
Entire Article

Copyright © 1986 American Institute of Historic and Artistic Works