QUANTITATIVE STUDY: THE EFFECTS OF SIZED MATERIALS AND “DRYING TIME” IN THE USE OF LASCAUX 360 HV AS A LINING ADHESIVE

Danielle Allard, & Kenneth B. Katz




MATERIALS

Lascaux 360 HV

Fine Art Stretchers and Services, Inc., P.O. Box 38, 1064 62nd Street, Brooklyn, NY 11219

Polyester—Terry Polyester #39

P & S Textiles, Jordon Rd., Skaneateles Falls, NY 13153

Belgian Linen—1 × 2, plain weave, 8 threads/cm in warp, 15 threads/cm in weft.

REFERENCES

DianeFalvey, “Practical Cold Lining Developments in Skaneateles, New York.” ICOM Committee for Conservation, 7th Triennial Meeting, Copenhagen, 10–14 Sept. 1984, 84.2.12.

BentHacke, “Apparatus for Treatment of Paintings.” ICOM Committee for Conservation, 5th Triennial Meeting, Zagreb, 1978, 78/2/12.

Kenneth B.Katz, “The Quantitative Testing and Comparisons of Peel and Lap/Shear for Lascaux 360 HV and BEVA 371.” AIC Journal, Vol. 24, No. 2 (Spring 1985), 60–68.

V.R.Mehra “Dispersion as Lining Adhesive and its Scope.” IIC Preprints, Paris Congress, 2–8 Sept, 1984, 44–45.

V.R.Mehra, “Cold-Lining and the Care of the Paint-Layer in a Tripple-Stretcher System. Also: Answers to some Questions and Doubts about the Cold-Lining System.” ICOM Committee for Conservation, 5th Triennial Meeting, Zagreb, 1978, 78/2/5.

V.R.Mehra, “Cold Lining and its Scope: Some Case Histories.” ICOM Committee for Conservation, 7th Triennial Meeting, Copenhagen, 10–14 Sept. 1984, 84.2.31.

AlanPhenix and GerryHedley, “Lining without Heat or Moisture.” ICOM Committee for Conservation, 7th Triennial Meeting, Copenhagen, 10–14 Sept. 1984, 84.2.38.

E.DeWitte, S.Florquin and M.Goessens-Landrie, “Influence of the Modification of Dispersions on Film Properties.” IIC Preprints, Paris Congress: 2–8 Sept. 1984, pp. 32–35

GerryHedley and CarolineVillers, “Lining in 1984: Questionnaire Replies.” ICOM Committee for Conservation, 7th Triennial Meeting, Copenhagen, 10–14 Sept. 1984, 84.2.22.

A.Howells, G.Burnstock, G.Hedley and S.Hackney, “Polymer Dispersions Artificially Aged.” IIC Preprints, Paris Congress, 2–8 Sept. 1984, pp. 36–43.