JAIC 1988, Volume 27, Number 1, Article 3 (pp. 38 to 39)
JAIC online
Journal of the American Institute for Conservation
JAIC 1988, Volume 27, Number 1, Article 3 (pp. 38 to 39)

A NOTE ON THE TREATMENT OF TWO GELATIN SILVER PHOTOGRAPHS BY HAROLD EDGERTON FROM THE PORTFOLIO “SEEING THE UNSEEN”

Meredith Mickelson


ABSTRACT—Technical information about Filmoplast-P is discussed and a procedure for the removal of the yellowed tape is described.

Article Sections:

1. INTRODUCTION
2. TECHNICAL INFORMATION ON FILMOPLAST-P TAPE
3. REMOVAL OF THE FILMOPLAST-P TAPE
4. CONCLUSION
a: Notes
Entire Article

Copyright 1988 American Institute for Conservation of Historic and Artistic Works