A STUDY OF THE MATERIALS USED BY MEDIEVAL PERSIAN PAINTERS

NANCY PURINTON, & MARK WATTERS


ABSTRACT—The paper includes a comparison of information about pigments in the literature on Persian painting to an analysis of the pigments in a group of Persian paintings at the Los Angeles County Museum of Art. A description of the classical medieval Persian painting technique is given as it is described in the liteature.