JAIC 1995, Volume 34, Number 3, Article 2 (pp. 173 to 186)
JAIC online
Journal of the American Institute for Conservation
JAIC 1995, Volume 34, Number 3, Article 2 (pp. 173 to 186)

THE ROLE OF GELATIN IN PAPER PERMANENCE

TIMOTHY BARRETT, & CYNTHEA MOSIER



NOTES

1. The TAPPI sample size is 1 g. TAPPI oven-dry weight is calculated based on the moisture content of a separate 2 g specimen as determined in accordance with TAPPI 412 (TAPPI 1991c). Our results showed no significant differnce in the % hydroxyproline recovered from paper reference standards that had been dried at 105°C for 12 hours and those that had not been dried.

2. The TAPPI extract is filtered through hardened filter paper.

3. TAPPI hydrolysis conditions are overnight at 110°C.

4. Decolorization with activated charcoal is not used in the TAPPI procedure. Our results showed no significant loss of hydroxyproline from paper reference standards treated with charcoal when run against calibration curve standards made from the same gelatin used to size the paper reference standards.

5. TAPPI evaporation is done at 110°C under nitrogen. We found no significant difference in % hydroxyproline measured in hydroxyproline solutions evaporated under house air at 100-105°C and reconstituted with water and tubes containing the same solutions and not evaporated at all.

6. TAPPI calibration curve hydroxyproline standards are not frozen. Our results showed no significant difference in the absorbances of hydroxyproline standards that had been stored frozen and those that had not. Percent recovery of hydroxyproline from the paper reference standards continued to be similar throughout the batches run, averaging 96 ± 5% over the course of the experiment. Had the concentration of the calibration curve standards been changing, this recovery calculation would have so indicated.

7. The TAPPI procedure requires that three reference standards be tested in triplicate each time a batch is run. The reference standard is a solution of the same glue used to size the paper being analyzed if possible. Otherwise, good-grade hide glue or purified calfskin gelatin are recommended. There is no procedure for preparing paper reference standards. Because we modified early steps, we felt that paper reference standards were necessary in order to monitor the entire procedure.



REFERENCES

Armstrong, W. G., and L.B.H.Tarlo. 1966. Amino acid components in fossil calcified tissues. Nature210:481–82.

Barrett, T.1989. Early European papers/contemporary conservation papers. The Paper Conservator13:1–108.

Barrett, T.1992. Evaluating the effect of gelatin sizing with regard to the permanence of paper. In Conference papers Manchester 1992, ed.S.Fairbrass. Manchester: Institute of Paper Conservation. 228–33.

Barrow, W.J.1972. Manuscripts and documents: Their deterioration and restoration. Charlottesville, Va.: University Press of Virginia. 35–37.

Barrow, W. J.1974. Physical and chemical properties of book papers 1507-1949. Richmond, Va.: W.J. Barrow Research Laboratory.

Courts, A.1980. Properties and uses of gelatin. InApplied protein chemistry, ed.R.A.Grant. London: Applied Science Publishers. 1–29.

Erickson, H.1994. Personal communication. Graduate School of Library and Information Studies, University of Texas at Austin, Austin, Tex. 78712

Finch, C.A., and A.Jobling. 1977. The physical properties of gelatin. In The science and technology of gelatin, ed.A. G.Ward and A.Courts. London: Academic Press. 249–94.

Hare, P.E.1969. Geochemistry of proteins, peptides and amino acids. In Organic geochemistry, ed.G.Eglinton and M.T.J.Murphy. Berlin: Springer-Verlag. 438–63.

Ho, T.1965. The amino acid composition of bone and tooth proteins in the late Pleistocene mammals. Proceedings of the National Academy of Sciences54: 26–31.

Inaba, M., and R.Sugisita. 1988. Permanence of washi (Japanese paper). In Preprints of the contributions to the Kyoto Congress, 19–23 September 1988, ed.J.Mills et al. London: International Institute for Conservation of Historic and Artistic Works. 1–4.

Leach, A. A., and J. E.Eastoe. 1977. The chemical examination of gelatins. In The science and technology of gelatin, ed.A.G.Ward and A.Courts. London: Academic Press. 475–506.

Rasch, R. H.1929. A study of purified wood fibers as a papermaking material. Bureau of Standards Journal of Research3(February):469–506.

Rasch, R. H.1931. Accelerated aging test for paper. Bureau of Standards Journal of Research7:465–75.

Rasch, R. H., M. B.Shaw, and G.W.Bicking. 1931. Highly purified wood fibers as papermaking material. Bureau of Standards Journal of Research7(August):765–82.

Rasch, R.H., M. B.Shaw, and G. W.Bicking. 1933. A study of some factors influencing the strength and stability of experimental papers made from two different sulphite pulps. Bureau of Standards Journal of Research11(July): 7–23.

Swartz, J.1994. Personal communication. Grinnell College, Department of Chemistry, Grinnell, Iowa 50112.

TAPPI. 1991a. Glue in paper (qualitative and quantitative determination). T504 om-89. In TAPPI Test Methods 1991. Atlanta, Ga.: Technical Association of the Pulp and Paper Industry.

TAPPI. 1991b. Organic nitrogen in paper and paperboard. T418 om-90. In TAPPI Test Methods 1991. Atlanta, Ga.: Technical Association of the Pulp and Paper Industry.

TAPPI. 1991c. Moisture in paper and paperboard. T412 om-90. In TAPPI Test Methods 1991. Atlanta, Ga.: Technical Association of the Pulp and Paper Industry.

Wilson, W. K., and E.J.Parks. 1980. Comparison of accelerated aging of book papers in 1937 with 36 years natural aging. Restaurator4(1):1–55.

Wilson, W. K., and E.J.Parks. 1983. Historical survey of research at the National Bureau of Standards on materials for archival records. Restaurator5(3–4):191–241.


AUTHOR INFORMATION

TIMOTHY BARRETT is an associate research scientist at the University of Iowa Center for the Book (UICB). As program director for UICB Paper Facilities, his duties include teaching papermaking history and technique at the School of Art and Art History and overseeing research and conservation paper production at a separate center facility. Address: UICB Paper, M109 Oakdale Hall, University of Iowa, Iowa City, Iowa 52242.

CYNTHEA MOSIER received a B.A. in biology from the University of California at Santa Cruz in 1971. Between 1972 and 1988 she served as staff research associate, Chemistry Board of Studies, at the same university. She studied under Timothy Barrett in the classroom for one year and worked as his research associate for an additional year. She is currently an apprentice in book and paper conservation under Pamela Spitzmueller in the Book Conservation Laboratory, University Libraries, University of Iowa.

This paper was presented at the 1994 AIC annual meeting, Book and Paper Specialty Group session, as “The role of gelatin in paper permanence 2” and published in the 1994 AIC Book and Paper Group Annual under the same title. The present version includes additions and revisions. The first work by Barrett on essentially the same topic is listed in the References above (Barrett 1992).


Copyright © 1995 American Institute for Conservation of Historic and Artistic Works