JAIC 1996, Volume 35, Number 1, Article 4 (pp. 45 to 59)
JAIC online
Journal of the American Institute for Conservation
JAIC 1996, Volume 35, Number 1, Article 4 (pp. 45 to 59)

GAS CHROMATOGRAPHIC ANALYSIS OF AMINO ACIDS AS ETHYL CHLOROFORMATE DERIVATIVES.

MICHAEL R. SCHILLING, HERANT P. KHANJIAN, & LUIZ A. C. SOUZA



3 RESULTS

Complete procedures for vapor-phase hydrolysis of proteins, derivatization of amino acids using ECF, and GC analysis with splitless injection and flame ionization detection (FID) are outlined in appendix 2. Information required to keep the procedure working reliably on a daily basis is described in appendix 3. Figure 1, an overlay of the analytical results for the amino acid calibration standard and a blank, shows that all the ECF-derivatized amino acids are resolved well. Although detection of histidine, tyrosine, and cysteine was possible, peaks for these amino acids do not exhibit the reproducibility required for proper quantitation. As stated earlier, because arginine does not derivatize by ECF, it cannot be detected. Figure 2 shows the chromatograms resulting from the analysis of whole egg, rabbit skin glue, and casein.

Fig. 1. Capillary gas chromatograms (scaling arbitrary) for ECF-derivatives of amino acids present in the Sigma A2161 calibration standard, and the analysis of an empty vial that served as a blank. The peaks for lysine (K), histidine (H), and tyrosine (Y) are indicated for the standard. Peaks for the remaining amino acids are identified in figure 2.

Fig. 2. Capillary gas chromatograms (scaling arbitrary) for ECF-derivatives of amino acids present in hydrolysates of whole egg, rabbit skin glue, and casein. Peaks for amino acids are labeled according to the list of abbreviations in appendix 1. The peak for lysine at 15.3 minutes was not shown to permit better clarity. Peaks for ethyl esters of azelaic acid, palmitic acid, stearic acid, and oleic acid appear in the chromatogram for whole egg at 6.35, 6.5, 7.18, and 7.27 minutes, respectively.

All protein amino acid compositions reported in tables 1, 2, and 3, including those obtained from the literature, are expressed in mole percent of only those amino acids detected by the ECF method. In addition, the weight percent of protein present in the samples could be estimated from the sum of the weight percentages of all ECF-derivatized amino acids detected. To correct for losses in the hydrolysis reaction, the weight percent of protein was normalized to the yield obtained for a sample of rabbit skin glue that was included in a separate vial with each set of sample vials. Typical hydrolysis yields for rabbit skin glue were 85–95% of all ECF-derivatized amino acids detected. The recovery of norleucine internal standard was also calculated in order to monitor transfer losses and solvent volume changes.

TABLE 1 AMINO ACID COMPOSITION DATA FROM VARIOUS SOURCES FOR SELECTED PROTEINS

TABLE 2 AMINO ACID COMPOSITION DATA FROM VARIOUS SOURCES FOR SELECTED EGG PROTEINS

TABLE 3 AMINO ACID COMPOSITION DATA FROM VARIOUS SOURCES FOR SELECTED PROTEINS

Table 1 summarizes the amino acid composition data for casein, glue, and gelatin samples. Data for egg proteins are listed in table 2. The results for blood, plant gums, other proteins, and proteinaceous contaminants are listed in table 3. In general, although the data listed in tables 1, 2, and 3 were acquired using several different analytical techniques, surprisingly good agreement was demonstrated. This fact illustrates that all the analytical techniques work well for pure, unpigmented samples of fresh protein.

Interesting results were obtained from the analysis of common plant gums (see table 3). All gums tested contained low levels of amino acids. Furthermore, low norleucine internal standard recoveries were consistent with observations that condensation products can form between the carbohydrates and the free amino acids, reducing overall yields (White 1984). However, the most significant observation was that hydroxyproline was present in every gum tested, in concentrations of up to 29 mole percent for samples of gum arabic.


Copyright © 1996 American Institute for Conservation of Historic and Artistic Works