PAINT DRIERS DISCUSSED IN 19TH-CENTURY BRITISH OIL PAINTING MANUALS
LESLIE CARLYLE
NOTES
1. The term media is being used here to conform to JAIC style. However, the author prefers the term mediums.
2. Some years ago two 19th-century oil paintings exhibiting disrupted surface textures that could correspond to this description of “seeding” were studied at the Canadian Conservation Institute (CCI). In both, many tiny inclusions in the paint could be seen, which were responsible for the texture effects. These particles were identified as consisting primarily of lead soaps (CCI 1992). Since the mechanism for their formation was not established, it was not clear whether lead based driers were responsible for this defect. Recently, similar inclusions in Rembrandt's Anatomy Lesson of Dr. Nicholas Tulp (1632, Mauritshuis, The Hague) have been investigated where lead soaps, fatty acids, diacids and a large quantity of lead chloride hydroxide were found in the inclusions. Researchers (Noble and Wadum 1998) hypothesize that treatments on linseed oil to render it more drying could be responsible. Further research is needed to establish whether the 19th-century inclusions which are morphologically very similar to those found in the Rembrandt result from the same mechanism. See also Campbell 1997.
REFERENCES
An American Artist [Laughton Osborn]. 1845. Handbook of young artists and amateurs in oil painting. New York: Wiley and Putnam.
Budavari et al., eds.1989. The Merck index, an encyclopedia of chemicals, drugs, and biologicals. 1989. 11th ed.Rahway, N.J.: Merck & Co.851.
BurnetJ.1861. Landscape painting in oil colours, explained in letters on the theory and practice of the art. Ed.H.Murray. London: James S. Vertue.
Campbell, R.1997. Possible evidence of 'seeding' in a seventeenth-century painting. Picture restorer12 (Autumn):11–12.
CCI. 1992Analytical research laboratory reports 3017.1, 3017.2. Canadian Conservation Institute, Ottawa, Canada.
CarlyleL.1991. A critical analysis of British handbooks, manuals and treatises on oil painting published in Britain between 1800–1900: With reference to selected eighteenth century sources. Ph.D. diss., Courtauld Institute of Art, University of London.
Carlyle, L., and TownsendJ.1990. An investigation of lead sulfide darkening of 19th century painting materials. Dirt and pictures separated preprints. London: United Kingdom Institute of Conservation. 40–43.
Cawse, J.1840. The art of painting portraits, landscapes, animals, draperies, satins, etc. in oil colours. London: Rudolph Ackermann.
Church, A. H.1890. The chemistry of paints and painting. London: Seeley, Service and Co.
Church, A. H.1901. The chemistry of paints and painting. London: Seeley, Service and Co.
Church, A. H.1915. The chemistry of paints and painting. London: Seeley, Service and Co.
A compendium of colours, and other materials used in the arts. 1808. London: C. Taylor.
Dossie, R.1758. The handmaid to the arts, vol. I. London: J. Nourse.
Dunn, Jr., E. J.1973. White hiding lead pigments. In Pigment handbook, properties and economics, ed.T. C.Patton, vol. 1. New York: John Wiley and Sons. 66.
Dunn, Jr., E. J.1975. Lead pigments. In Treatise on coatings, pigments, pt. 1, vol. 3, ed.R. R.Myers and J. S.Long. New York: Marcel Dekker. 403–4.
Eastlake, Sir Charles. 1847. Materials for a history of oil painting, vol. 1. London: Longman, Brown, Green and Longmans. 350. George Field's annotated copy is in the Canadian Conservation Institute Library.
Ellis, T. J.1897. Sketching from nature: A handbook for students and amateurs. London: Macmillan.
Elm, A. C.1934. A century of progress in driers. Industrial and engineering chemistry26:386–88.
Field, G.1835. Chromatography; or, A treatise on colours and pigments, and of their powers in painting. London: Charles Tilt.
Field, G.1841. Chromatography; or, A treatise on colours and pigments, and of their powers in painting. New ed.London: Tilt and Bogue.
Field, G.1850. Rudiments of the painter's art; or, A grammar of colouring applicable to operative painting, decorative architecture, and the arts. London: John Weale.
Fielding, T. H.1839. On painting in oil and water colours, for landscape and portraits. London: Ackermann & Co.
Hurst, G. H.1892. Painters' colours, oils, and varnishes: A practical manual. London: Charles Griffin & Company.
Ibbetson, J. C.1828. An accidence, or gamut of painting in oil, with a brief memoir of the author's life. London: Harvey and Darton.
Kirk-Othmer. 1981. Encyclopedia of chemical technology. 3d ed.New York: John Wiley & Sons. 14:169–70.
Laurie, A. P.1895. Facts about processes, pigments, and vehicles: A manual for art students. London: Macmillan and Co.
Lechertier, Barbe, & Co. 1870. List of colours and materials for tapestry painting, oil painting, &c. London: Lechertier, Barbe, & Co.
Martel, C.1859. On the materials used in painting, with a few remarks on varnishing and cleaning pictures. London: G. Rowney and Co.
Martens, C., ed.1974. Technology of paints, varnishes and lacquers. Rev. ed.New York: R. E. Krieger Publishing Company.
Merimée, J. F. L.1830. De la peinture à l'huile. Paris: Mme. Huzard.
Merimée, J. F. L.1839. The art of painting in oil, and in fresco, trans. W. B. Sarsfield Taylor. London: Whitakker & Co.
Neil, J. W.The art of making copal and spirit varnishes, &c. Transactions of the Society Instituted at London for the Encouragement of Arts, Manufactures, and Commerce, vol. XLIX. London, 1833:33–37.
Noble, P., and J.Wadum. 1998. The restoration of the 'anatomy lesson of Dr. Nicolaes Tulp.' In Rembrandt under the scalpel: The anatomy lesson of Dr. Nicolaes Tulp dissected, eds.M.Enklarr, P.van derPloeg. Amsterdam, The Hague: Mauritshuis/Six Art Promotion. 51–74.
A practical treatise on painting in oil-colours. 1795. London: B. and J. White.
Riffault, M., M.Vergnaud, and Toussaint, 1874. A practical treatise on the manufacture of colours for painting, ed.M. F.Malepeyre, trans. A. A. Fesquet. Philadelphia and London: Henry Carey Baird, Sampson Low, Marston, Low & Searle.
Roberson Archive, Hamilton Kerr Institute, Cambridge University, Whittlesford, Cambridge, England. Recipe book HKI MS 788–1993.
Scott Taylor, J.1890. Modes of painting described and classified. London: Winsor & Newton.
Smith, M.1693. The art of painting. London: Printed by M. B. for the author.
Standage, H. C.1892. The use and abuse of colours and media in oil painting: A handbook for artists and art students. London: Reeves & Sons.
Sully, T.1873. Hints to young painters, and the process of portrait painting as practiced by the late Thomas Sully. Philadelphia: J. M. Stoddard & Co.
Templeton, J. S.1849. The guide to oil painting. London: G. Rowney & Co.
Tingry, F.1804. The painter and varnisher's guide. London: G. Kearsley.
Townsend, J., L.Carlyle,A.Burnstock, M.Odlyha, and J.Boon. 1998. 19th-century paint media. Part I, The formulation and properties of megilps. IIC preprints: Painting techniques—History, materials and studio practice. Dublin: International Institute for Conservation of Historic and Artistic Works. 205–10.
Vibert, J. G.1892. The science of painting, trans. Percy Young. London: Percy Young.
Williams, W.1787. An essay on the mechanic of oil colour. Bath, England: W. Williams.
Winsor & Newton. 1900. Wholesale catalogue. For the trade only. London: Winsor & Newton.
AUTHOR INFORMATION
LESLIE CARLYLE has a B.A. in art history and theater arts from Queen's University, Kingston Ontario, 1973; a bachelor of fine arts (studio art), Concordia University, Montreal, Quebec, 1975; and a master of art conservation, Queen's University, Kingston, Ontario, 1979. She was assistant paintings conservator at the National Historic Parks and Sites from 1979 to 1980. She joined the Canadian Conservation Institute (CCI) as a paintings conservator in 1980. In 1987, she was granted educational leave to pursue a Ph.D. in the Technology and Conservation Department of the Courtauld Institute of Art in London. She resumed her position as paintings conservator with CCI in May 1991. She received her doctorate from the University of London in September 1991. In 1995, she transferred to the Conservation Processes and Materials Research Division at CCI in order to carry out research as a materials historian.
|