SALTS IN THE DETERIORATION OF POROUS MATERIALS: AN OVERVIEW

A. ELENA CHAROLA, & Herodotus


“I observed … that salt exuded from the soil to such an extent as even to injure the pyramids.”

—Herodotus, (484 B.C.–425 B.C.), History, bk. 2