THE SWELLING OF ARTISTS' PAINTS IN ORGANIC SOLVENTS. PART 1, A SIMPLE METHOD FOR MEASURING THE IN-PLANE SWELLING OF UNSUPPORTED PAINT FILMS
ALAN PHENIX
NOTES
1. The measurements from separate experiments can be considered as a sample from an infinite population of possible measurements; and, likewise, the means of any series of measurements are a sample from the possible means of samples of measurements from the whole population. The distribution of the sample means is called the sampling distribution of the mean: its mean is the same as the mean of the original population. The standard error of the mean (SEM) is equivalent to the standard deviation of the sampling distribution of the mean (Miller and Miller 1993).
REFERENCES
Barr-Howell, B. D., and N. A.Peppas1985. Dynamic and equilibrium swelling of DVB crosslinked polystyrene particles. Journal of Applied Polymer Science30:4583–89.
Bilson, T.1996. Canvas shrinkage: A preliminary investigation into the response of a woven structure. ICOM Committee for Conservation preprints, ed. J.Bridgland, 11th Triennial Meeting, Edinburgh. London: James and James. 1:245–52.
Bristow, G. M., and W. F.Watson1958. Cohesive energy densities of polymers. Part 1, Cohesive energy densities of rubbers by swelling measurements. Transactions of the Faraday Society54:1731–41.
Browne, F. L1956. Swelling of oil paints in water. Part 8, Swelling of linseed oil paints in water and organic liquids. Forest Products Journal6:312–18.
Brunt, N. A1964. Blistering of paint layers as an effect of swelling by water. Journal of the Oil and Colour Chemists' Association47:31–42.
Byun, J., Y. M.Lee, and C. S.Cho1996. Swelling of thermosensitive interpenetrating polymer networks composed of polyvinylalcohol and polyacrylic acid. Journal of Applied Polymer Science61(4):697–702.
Chen, W. L., K. R.Shull, T.Papatheodorou, D. A.Styrkas, and J. L.Keddie1999. Equilibrium swelling of hydrophilic polyacrylates in humid environments. Macromolecules32:136–44.
Down, J. L1999. Swelling as an indicator of removability. In Reversibility: Does it exist?ed. A.Oddy and S.Carroll. London: British Museum. 111–27.
Eissler, R. L., and L. H.Princen1968. Effect of some pigments on tensile and swelling properties of linseed oil films. Journal of Paint Technology40(518):105–11.
Eissler, R. L., and L. H.Princen1970. Swelling of linseed oil films in acid and alkaline environments. Journal of Paint Technology42(542):155–58.
Erhardt, D., and J-S.Tsang1990. The extractable components of oil paint films. In Cleaning, retouching, coatings, ed. J. S.Mills and P.Smith. London: International Institute for Conservation. 93–97.
Errede, L. A1992. Polymer swelling. Part 11, A molecular interpretation of association in polystyrene-liquid systems. Polymer33(19):2168–76.
Faraday Society1946. Swelling and shrinking: A general discussion.Edinburgh: Gurney and Jackson. (Reprint of the Transactions of the Faraday Society 42B [1946].)
Feller, R. L., N.Stolow, and E. H.Jones1985. On picture varnishes and their solvents. Rev. and enlarged ed. Washington, D.C.: National Gallery of Art.
Gee, G1942. The interaction between rubber and liquids. Part 3, The swelling of vulcanised rubber in various liquids. Transactions of the Faraday Society3:418–22.
Green, A., and G. I. P.Levenson1972. A practical swellmeter. Journal of Photographic Science20:205–10.
Hedley, G., M.Odlyha, A.Burnstock, C.Husband, and J.Tillinghast1990. A study of the mechanical and surface properties of oil paint films treated with organic solvents and water. In Cleaning, retouching, coatings, ed. J. S.Mills and P.Smith. London: International Institute for Conservation. 98–105.
Huglin, M. B., and D. J.Pass1968. Cohesive energy density of polytetrahydrofuran. Journal of Applied Polymer Science12:473–85.
Johnsen, J. S1996. Accelerated aging: Changes in swelling and melting point of photographic gelatin. ICOM Committee for Conservation preprints, ed. J.Bridgland, 11th Triennial Meeting, Edinburgh. London: James and James. 2:586–90.
Lewis, E. J., and A. K.Soper1950. Note on an apparatus for measuring the vertical swelling of colloid layers. Journal of Scientific Instruments31(27):242–43.
Long, J. S., S.Thames, and O.Smith1967. Surface forces and dimensions. Journal of Paint Technology39(507):169–81.
Mangaraj, D1963. Cohesive energy densities of high polymers. Part 1, Determination of cohesive energy density from swelling measurements. Makromolekulare Chemie65:29–38.
Michalski, S1990. A physical model of the cleaning of oil paint. In Cleaning, retouching, coatings, ed. J. S.Mills and P.Smith. London: International Institute for Conservation. 85–92.
MillerJ. C., and J. N.Miller1993. Statistics for analytical chemistry.3d ed.London: Ellis Horwood.
Morehead, F. F1952. A method for studying the effect of humidity on the cross-sectional swelling of some common fibers. Textile Research Journal22:535–39.
Nguyen, T.-P., B.Lavedrine, and F.Flieder1999. Effets de la pollution atmosphérique sur la dégradation de la gélatine photographique. ICOM Committee for Conservation preprints,ed. J.Bridgland, 12th Triennial Meeting, Lyons. London: James and James. 2:567–71.
Parbhoo, B., S.Izrael, J. M.Salamanca, and J. L.Keddie. 2000. Use of ellipsometry and gravimetry to develop standards for measuring silicone coat weight and thickness with x-ray fluorescence spectroscopy. Surface and Interface Analysis29:341–45.
Parker, L. V., and T. A.Ranney1995. Additional studies on the softening of rigid PVC by aqueous solutions of organic solvents. U.S. Army Corps of Engineers, Cold Regions Research and Engineering Laboratory. Special report 95-8.
Parker, L. V., and T. A.Ranney1996. Further studies on the softening of rigid PVC by aqueous solutions of organic solvents. U.S. Army Corps of Engineers. Cold Regions Research and Engineering Laboratory. Special report 96-26.
Peppas, N. A., and E. W.Merrill1976. Determination of interaction parameter χ1 for poly (vinyl alcohol) and water in gels crosslinked from solutions. Journal of Polymer Science, Polymer Chemistry Edition14:459–64.
Phenix, A1998. Solvent-induced swelling of paint films: Preliminary results. Western Association for Art Conservation Newsletter20(3):15–20.
Phenix, A.2002. The swelling of artists' paints in organic solvents. Part 2, Comparative swelling powers of selected organic solvents and solvent mixtures. Journal of the American Institute for Conservation41:61–90.
Rinse, J., and W. H. G.Wiebols1937. Swelling of drying oil films in water. Industrial and Engineering Chemistry29(10):1149–54.
Salomon, G., and G. J.van Amerongen1947. Influence of structure on polymer-liquid interaction. Part 1, Relative and absolute values of swelling equilibria. Journal of Polymer Science2:355–70.
Scott, R. L., and M.Magat1949. Thermodynamics of high polymer solutions. Part 3, Swelling of cross-linked rubber. Journal of Polymer Science4:555–71.
Stolow, N1954. A modified apparatus for measuring the swelling of polymer films in solvents. Journal of Scientific Instruments31:416–20.
Stolow, N1955. Some investigations of the action of solvents on drying oil films. Ph.D. diss., Courtauld Institute of Art, University of London.
Stolow, N1963. Application of science to cleaning methods: Solvent action studies on pigmented and unpigmented linseed oil films. In Recent advances in conservation, ed. G.Thomson. London: Butterworths. 84–88.
Tan, N. C. B., W. L.Wu, W. E.Wallace, and G. T.Davis1998. Journal of Polymer Science, Part B: Polymer Physics36:155.
Thiessen, P. A1925. Methoden zur quantitativen Bestimmung von Quellungsgrößen. Kolloid Zeitschrift37:406–11.
Zellers, E. T., D. H.Anna, R.Sulewski, and X.Wei1996a. Critical analysis of the graphical determination of Hansen's solubility parameters for lightly crosslinked polymers. Journal of Applied Polymer Science62:2069–80.
Zellers, E. T., D. H.Anna, R.Sulewski, and X.Wei1996b. Improved methods for the determination of Hansen's solubility parameters and estimation of solvent uptake for lightly crosslinked polymers. Journal of Applied Polymer Science62:2081–96.
AUTHOR INFORMATION
ALAN PHENIX was educated at Leeds University, United Kingdom, receiving a B.Sc. Honors in chemistry and color chemistry combined in 1979. He studied conservation of easel paintings for three years at the Courtauld Institute of Art, University of London, and was awarded the institute's postgraduate diploma in 1984. After an internship at Tate Gallery, London, he worked as a paintings conservator in Australia, returning to Britain in 1989 to take up a teaching and research position at the Hamilton Kerr Institute, University of Cambridge. He was a lecturer in the Department of Conservation and Technology at the Courtauld Institute of Art from 1991 to 2000, during which time he spent 15 months on secondment to the MOLART (Molecular Aspects of Aging in Painted Works of Art) project managed by the Foundation for Fundamental Research on Matter, Institute for Atomic and Molecular Physics (FOMAMOLF), Amsterdam. During 2001 he was research fellow at the Royal College of Art, London, and he has recently been appointed associate professor at the Institute for Archaeology, Art History and Conservation, at the University of Oslo. He is presently coordinator of the ICOM-CC Working Group Paintings 1: Conservation and Restoration of Paintings. Address: Department of Conservation Studies, Institute for Archaeology, Art History and Conservation (IAKK), University of Oslo, Frederiks gt. 3, 0164 Oslo, Norway.
|