JAIC 2005, Volume 44, Number 1, Article 2 (pp. 13 to 26)
JAIC online
Journal of the American Institute for Conservation
JAIC 2005, Volume 44, Number 1, Article 2 (pp. 13 to 26)

ANALYSIS OF LAMINATED DOCUMENTS USING SOLID-PHASE MICROEXTRACTION

Mark Ormsby




REFERENCES

Ballany, J., D.Littlejohn, R. A.Pethrick, and A.Quye. 1998. Probing the factors that control degradation in museum collections of cellulose acetate artefacts. In Historic textiles, papers, and polymers in museums, ed. J. M.Cardamone and M.Baker. American Chemical Society Symposium series 779, vol. 12. Washington, D. C.: American Chemical Society. 145–165.

Barrow, W. J.1965. Deacidification and lamination of deteriorated documents, 1938–1963. American Archivist28(2): 285–90.

Chemfate. 2004. Environmental Fate Database. Syracuse Research Corporation. www.syrres.com/esc/chemfate.htm (accessed June 2004).

Clements, R. F.1972. Accelerated aging of cellulose acetate lamination films. Research and Testing Laboratory, National Archives and Records Administration, Washington, D. C.

Conley, J.1998. Using LC-MS to preserve a national treasure. Today's Chemist at Work7(2): 43–46.

DeCroes, G. C., and J. W.Tamblyn. 1952. Protection of cellulose esters against breakdown by heat and light. Modern Plastics29:27–189.

Ferrari, F., A.Sanusi, M.Millet, and M.Monturyl. 2004. Multiresidue method using SPME for the determination of various pesticides with different volatility in confined atmospheres. Analytical and Bioanalytical Chemistry379(3): 476–83.

Gear, J. L.1957. Comments on Mr. Turner's article. American Archivist20(4): 329–34.

Gear, J. L.1965. Lamination after 30 years: Record and prospect. American Archivist28(2): 293–97.

George, C., and H.Prest. 2002. Determination of phthalate esters by positive chemical ionization MS with retention-time locked GC. LCGC North America20(2). www.chromatographyonline.com (accessed September 2003).

Glastrup, J.1995. Analysis of gaseous degradation products generated during accelerated aging of cellulose acetate. Research techniques in photographic conservation: Proceedings of the Conference in Copenhagen. Copenhagen: Academy of Fine Arts. 93–95.

Haslam, J., and H. A.Willis. 1965. Identification and analysis of plastics. Princeton, N. J.: D. Van Nostrand.

Hites, R. A.1997. Gas chromatography mass spectrometry. In Handbook of instrumental techniques for analytical chemistry, ed. F.Settle. Upper Saddle River, N. J.: Prentice Hall. 609–26.

Kumar, R.1999. A mass spectral guide for quick identification of phthalate esters. American Laboratory31(November): 32–35.

Lattuati-Derieux, A., S.Bonnassies-Termes, and B.Lavedrine. 2004. Identification of volatile organic compounds emitted by a naturally aged book using solid-phase microextraction/gas chromatography/ mass spectrometry. Journal of Chromatography A1026:9–18.

Maines, C.2002. Analysis of exhibition materials. Paper presented at the Eastern Analytical Symposium, Somerset, N. J.

Page, S.2003. Cellulose acetate lamination at the National Archives. Part 1: The Louisiana Purchase documents: A case study. In Book and Paper Group Annual22. American Institute for Conservation Book and Paper Group. Washington, D. C.: AIC. 53–59.

Pawliszyn, J.1998. Solid phase microextraction: Theory and practice.New York: John Wiley & Sons.

Pawliszyn, J. ed.1999. Applications of solid phase microextraction. Cambridge: Royal Society of Chemistry.

Penalver, A., E.Pocurull, C.Aguilar, F.Borrull, and R. M.Marce. 2000. Comparison of different fibers in the solid phase microextraction of phthalate esters from water samples. Journal of Chromatography A922(1–2): 377–84.

Rhyl-Svendsen, M.2003. Home page of the Indoor Air Pollution Working Group. http://iaq.dk/iap.htm (accessed September 2003).

Rhyl-Svendsen, M., and J.Glastrup. 2002. Acetic acid and formic acid concentrations in the museum environment measured by SPME–GC-MS. Atmospheric Environment36:3909–16.

Shashoua, Y. R.2001. Inhibiting the deterioration of plasticized poly(vinyl chloride): A museum perspective. PhD diss., Technical University of Denmark, Copenhagen. www.natmus.dk/cons/reports/2001/ys_phd/pvcphd.htm (accessed September 2003).

Shinagawa, Y., M.Murayama, and Y.Sakaino. 1992. Investigation of the archival stability of cellulose triacetate film: The effects of additives to CTA support. In Polymers in conservation, ed. N. S.Allen, M.Edge, and C. V.Horie. Cambridge: Royal Society of Chemistry. 138–50.

Stannett, V.1950. Cellulose acetate plastics. London: Temple Press.

Staples, C. A., D. R.Peterson, T. F.Parkerton, and W. J.Adams. 1997. The environmental fate of phthalate esters: A literature review. Chemosphere35(4): 667–749.

Stiber, L.1988. The delamination of the Washington and Lee ledger. Part 1: An overview of cellulose acetate lamination. In Early Advances in Conservation, ed.V.Daniels. British Museum Occasional Papers 6. London: British Museum. 27–40.

Supelco. 1999. Solid phase microextraction: Theory and optimization of conditions. Bulletin 923A. Supelco, Bellefonte, Pa.

Supelco. 2001. Solid phase microextraction troubleshooting guide. Bulletin 928. Supelco, Bellefonte, Pa.

Supelco. 2002. Solid phase microextraction application guide CD, 4th ed. Supelco, Bellefonte, Pa.

Vas, G., and K.Vekey. 2004. Solid-phase microextraction: A powerful sample preparation tool prior to mass spectrometric analysis. Journal of Mass Spectrometry39:233–54.

Williams, R. S.1993. Composition implications of plastic artifacts: A survey of additives and their effects on the longevity of plastics. In Saving the twentieth century: The conservation of modern materials,ed. D. W.Grattan. Ottawa: Canadian Conservation Institute. 135–53.

Wilson, A. S.1995. Plasticizers: Principles and practice. London: Institute of Materials.

Wilson, W. K., and B. W.Forshee. 1955. Preservation of documents by lamination. National Bureau of Standards, report 4207 to National Archives and Records Service. Washington, D. C.

Wilson, W. K., and B. W.Forshee. 1959a. Degradation of cellulose acetate films. Society for Plastics Engineers Journal15: 146.

Wilson, W. K., and B. W.Forshee. 1959b. Preservation of documents by lamination.National Bureau of Standards Monograph. Washington, D. C.: Government Printing Office.

Wilson, W. K., and E. J.Parks. 1983. Historical survey of research at the National Bureau of Standards on materials for archival records. Restaurator5(34): 191–241.



SOURCES OF MATERIALS

SPME fibers, inlet liners, and vials

Supelco 595 North Harrison Rd. Bellefonte, Pa. 16823-0048 (800) 247-6628 www.sigma-aldrich.com/supelco

GC-MS and HP5-MS column

Agilent Technologies 2850 Centerville Rd. Wilmington, Del. 19808 (800) 227-9770 www.agilent.com/chem

8061 Phthalates Standard Mixture

NSI Solutions, Inc. 7517 Precision Dr., Suite 101 Raleigh, N.C. 27617 (800) 234-7837


AUTHOR INFORMATION

MARK ORMSBY graduated from Grinnell College, Grinnell, Iowa, with a degree in physics and received an MS in physics from the University of Maryland. Since 1990 he has worked at the National Archives and Records Administration, initially focusing on conservation applications of image processing. His current research interests include environmental monitoring, studying the role of gelatin sizing in paper degradation, and developing new applications of SPME–GC-MS. Address: National Archives and Records Administration, 8601 Adelphi Rd., Room 1800, College Park, Md. 20740–6001


Copyright © 2005 American Institution for Conservation of Historic & Artistic Works