Brown, JP
The Field Museum Archaeological Metals Project: Distributed, In Situ Micro-Environments for the Preservation of Unstable Archaeological Metals Using Escal® Barrier Film.


Delidow, Margo and Cynthia Albertson
Re-thinking the Cleaning of Claes Oldenburg’s Floor Cake


el-Serogy, Abdel-Rahman and Abdel-Salam Eleasely
Conservation and Restoration of an Egyptian Wooden Human-Like Form Coffin in Suez Museum


Garland, Kathleen M. and John Twilley
The Restoration, Treatment, Scientific Examination and Re-Treatment of an Egyptian Limestone Relief from the Tomb of Ka-Aper


Gunnison, Anne Turner, Susan Heald, Jia-Sun Tsang, and Yoonjo Lee
Preventive Conservation and Identification of Plastics of a Recent Acquisition at the National Museum of the American Indian


Hargrove, Suzanne
Keeping the Circle Unbroken: Treatment of David Smith’s 2 Circle IV


Krueger, Robert
A New Approach to Maintaining Water Features and Eliminating Re-occurring Biological Growth Outbreaks


Ly, Tin
Emerald Laser Lawn by Dan Corson in the Broward County Public Art and Design Collection


Mardikian, Paul
Resurrecting a Set of Composite Tools from the 1st Century A.D. Roman Wreck of Porto-Novo, Corsica, France


Posner, Katrina
Henry Moore's Bronze Form: Investigating the Original Patina


Senge, Dana K. and Ellen Carrlee
Examining Past Treatments of Waterlogged Basketry from the Pacific Northwest and Alaska


Smith, Andrew
Inside Out, Red, The Conservation of an Anish Kapoor Powder-Pigment Sculpture


Stein, Renée, Susan Blevins, Nelson Burke, Dr. David Rosen and Andrew Layton
Using 3-D Prototyping as an Intermediary in the Reconstruction of Ancient Pottery


Thompson, Mina and Conor McMahon
Plaster, Pliacré® and Paper


Wheeler, George, Carolyn Riccardelli, Christina Muir, George Scherer and Joe Vocaturo
An Examination of Pinning Materials for Marble Sculpture