antique marble

A series of marble patterns executed by dropping red, black 7 and yellow, or red, blue and yellow, on the marbling size, and raking once up and down; this is followed by an application of green coloring and, if the pattern is to be an antique spot, pink or green spots. Finally, there is a sprinkling of white. Other colors are also used. The antique marble is produced in a variety of patterns, including spots, straight, and curled. (369 )