back-molding iron

See illustration

An implement, usually made of iron, approximately 20 inches long, 6 inches wide and 2 1/2 inches thick, and used in forming the millboard for the SPRING-BACK of a book. The iron is made with several grooves of various widths on both sides. (264 )