Bagguley, Thomas

An English bookbinder, of Newcastle under Lyme, who, in the late 19th century, devised a method of tooling vellum and similar materials in permanent colors. Bagguley limited his technique to vellum, as he considered leather to be too lacking in purity of color to offer a satisfactory ground for unrestricted color decoration. Because of the delicate nature of his work, he further restricted his technique to vellum doublures. See also: SUTHERLAND DECORATION . (94 )