belly

The extreme left or right side of a complete hide, removed by cutting the hide along a line parallel to the spine and at such a distance from it as to remove approximately 23% of the total area of the hide for the two bellies. The belly includes the front and hind shank. The line of cutting is determined more accurately for any individual hide by noting the change in feel from the denser structure of the crop to the looser structure of the belly. (61 , 363 )