brokers

Binding agents, who were go-betweens or self-appointed salesmen of publishers or library binders, and who solicited binding business and then let out the work to the lowest-priced bidder on their list. Mason Locke Weems ("Parson Weems"), the creator of the George Washington cherry tree myth, seems to have been one such agent, working between binders and the publisher, Matthew Carey. Binding brokers, who flourished in the United States well into the 20th century, are rare today. (131 , 308 )