build in ( building in )

The process of placing newly cased-in library books between smooth or brass-bound boards and applying pressure in a standing press or hydraulic press, or applying dry heat and (considerable) pressure for a brief time (usually 8 to 15 seconds) in a hydro-press or BUILDING-IN MACHINE . Building in forms the joints, compresses the book, secures it firmly in its case and reduces substantially any possibility of board warpage. See also: CASING-IN . (139 )