calcium hypochlorite

Any hypochlorite of calcium, e.g., the normal anhydrous salt (Ca(ClO)2), that is generally found in commercial products containing 70 to 75% available chlorine. Calcium hypochlorite is used by many paper conservationists to bleach archival papers, and it is also used as an oxidizing agent to reduce the effects of FOXING . Its use is potentially harmful, as the chlorine is difficult to remove. Also known as "bleaching powder."