A WAX found as an exudate on the leaves and stems of a plant (Euphorbia antisyphilitica) found in northern Mexico and the southwestern United States, and obtained by boiling the leaves and stems with water and sulfuric acid. It is yellowish-brown in color and is opaque to translucent. It is classed as hard wax and has a softening range at 64 to 68° C. It is used in making varnish and as a substitute for CARNAUBA WAX to impart a high gloss to leathers that are not glazed. (291 )