A lightweight paper, either coated or with an
English finish, usually made with a considerable
proportion of mechanical pulp, and used for
mail-order catalogs, telephone directories, and
the like. Uniformity of weight, opacity. finish,
formation, and sufficient strength to get through
high-speed printing presses are desired
characteristics. Basis weights usually range from
19 to 28 pounds (24 X 36). (17 , 324 )