A cover marble executed by sprinkling black and
brown coloring on the covers, followed by orange
in various places to give a cloudlike effect. This
is followed by red placed near the orange. When
this is dry, the covers are coated two or three
times with yellow, which is allowed to penetrate
evenly into the leather. (97 , 152 )