cloth tooling

The process of tooling in gold on a cloth binding. As with leather, glair is required, and, in addition, greater pressure is required because the surface of cloth is harder, especially the surface of a filled cloth. Pyroxylin impregnated cloth or imitation leather sometimes has to be washed with methylated spirits before being tooled. (54 )