coated

Paper or board which has had its surface modified by the application of clay or other pigment and adhesive materials, or other suitable material, with the intent of improving its finish in terms of printability, color, smoothness, opacity, etc. The term is also applied to lacquered or varnished papers and book cloth, as well as other covering materials.