finisher

1. The bookbinder or gilder who performs the processes of polishing the leather, lettering. and embellishing, which are carried out on a hand-bound book subsequent to forwarding. In France, it is not unusual for the two operations—i.e., forwarding and finishing—to he performed by different persons: in England and the United States. on the other hand, the two are usually done by the same craftsman. except in commercial hand binding. 2. A machine used to apply varnish, lacquer, or other fluid to covering materials by means of a spray or roller, or a printing or blocking plate. 3. A term sometimes applied to flat or cylindrical polishing tools, e.g., a BURNISHER (2) . (158. 173 )