gas black

A black pigment used in the manufacture of printing ink, and produced by burning gas with insufficient oxygen for complete combustion to take place. Thick soot is deposited on metal cylinders in much the same manner as LAMPBLACK from oil. Gas black is practically pure carbon. (140 )