gilder's tip

A camel-hair brush about 3 to 4 inches in width, and used to pick up strips of gold leaf flat on the tips of the hairs. A tip of long hairs is used to pick up whole leaves, while one with short hairs is used for cut pieces of leaf. A tip is not usually needed for metal leaf that is heavier and easier to handle than gold, but one may be necessary for silver leaf, in which case a special tip with double thickness of hairs is used. (233 , 335 )