gloss ( glossiness )

The surface characteristic of a material which enables it to reflect light specularly and which causes it to appear shiny or lustrous. Gloss is measured at various angles of illumination, and, although it is subjective in nature, it is clearly associated with the light reflecting properties of a surface. (17 )