gold cushion

A pad on which a sheet of gold leaf is placed for cutting the pieces required for tooling. It usually consists of a piece of wood padded with blotting paper, cotton wool, or the like, and covered with calfskin, flesh side out, and powdered with brick dust. A stiff piece of paper is sometimes attached to the rear edge, and run around the sides to enclose about one-third of the cushion, as a sort of windshield to protect the fragile leaves from air currents. (233 , 335 , 343 )