hand sizing

A method of sizing or resizing paper by dipping the sheets or leaves into a tub of size. Hand sizing was the original method of sizing paper, i.e., handmade paper, and is still used for that class of paper, and also by restorers when resizing documents or the leaves of a book. Old papers, which often contain decomposed size, can be made stronger and safer to handle if resized by hand. (77 , 197 )