hard glue

A GLUE used in the past in machine case-making where quick setting was the principal requirement of the glue and minimum flexibility was not a serious disadvantage. Such glues are hard in the sense that they contain no plasticizer. They were not used for gluing-up the spine, lining-up, or for flexible cover making, and are now seldom used in book production for any purpose. (256 )