hinged boards

A type of binding having boards attached to a stab-sewn or post binding, by means of a cloth hinge which joins the main board to a narrow board at the spine of the book. The narrow board is secured by the posts or stab sewing. Hinged boards are characteristic of some types of blankbooks. (119 , 204 )