Bookbinding and the Conservation of Books
A Dictionary of Descriptive Terminology

 Previous item  Up One Level Next item

hung on guards

Inserts, such as maps, plates, etc., which have been glued to strips of paper or linen, which are then tipped or stubbed into the book (256 )