The skin of the herbivorous marsupials (family Macropodidae) of Australia, New Guinea, etc., which when properly tanned, makes a supple and durable bookbinding leather. Today, it is generally chrome tanned with a glazed finish, thus making it unsuitable for use as a bookbinding leather. It is said to be stronger, weight for weight, than any other leather. (325 )