leather marble

A method of coloring leather so as to obtain something of a marbled effect. The skins are dampened and rolled into a ball, each skin being carefully arranged so that no large area of any one is hidden in the folds. The ball of skins is then immersed in the dye, which colors the skins at the edges only, resulting in a kind of marbling effect. (164 )