library buckram

1. A heavy weight cotton fabric possessing the qualities called for in the minimum specifications for Class "A" library binding. See also: BOOK CLOTH ;BUCKRAM . 2. A trade name sometimes incorrectly applied to all book cloths of a similar nature, e.g., all coated cloths, all impregnated cloths, etc.