Pebbling is often employed to improve the appearance, bulk, or pliability of paper so that a cheaper paper may be substituted for more expensive stock.
It may be used to finish small quantities of paper which otherwise could not be purchased with a pebbled finish except in large quantities. (234 , 278 )