Bookbinding and the Conservation of Books
A Dictionary of Descriptive Terminology
scrow
Strips, clippings, or other waste parts of hide or skin used in the manufacture of glue, and at one time used by papermakers as a source of animal gelatin for sizing paper. (
197
)