veal

A leather produced with a grain pattern similar to, but somewhat coarser than, calfskin, and made from the skins of immature bovine animals which have not been fed on grass subsequent to weaning. The animals are allowed to grow to a comparatively large size, yielding skins larger and heavier than calfskins but smaller than cowhides. See also: KIP (2) . (61 )