zinc sulfide

A compound (ZnS), which occurs naturally as "blende," and is prepared directly from the elements and by precipitation of a zinc salt solution with ammonium sulfide. It is used as a pigment, or as a component ofLITHOPONE as a loading material or coating pigment in the manufacture of paper. (17 )