JAIC 1979, Volume 18, Number 2, Article 1 (pp. 61 to 81)
JAIC online
Journal of the American Institute for Conservation
JAIC 1979, Volume 18, Number 2, Article 1 (pp. 61 to 81)

THE EFFECTS OF WASH WATER QUALITY ON THE AGING CHARACTERISTICS OF PAPER

Lucia C. Tang, & Norvell M. M. Jones




REFERENCES

Hey, M.Report to the Council on Library Resources, (Grant CLR-536). Unpublished (1974).

Santucci, L.Problems of Conservation in Museums. Paris: ICOM, p. 187–207 (1969).

Williams, J. C., Fowler, C. S., Lyon, M. S. and Merrill, T. L.Advances in Chemistry Series. Washington, D.C.: American Chemical Society, No. 164, p. 37–61 (1977).

Cellulose Conference, University of California, 1974. Cellulose as a Chemical and Energy Resource. N.Y: Wiley(1975).

Clapp, A. F.Curatorial Care of Works of Art on Paper. Oberlin: Intermuseum Conservation Association (1974).

Barrow, W. J. “A Two Year Research Program,” Permanence/Durability of the Book. Richmond, Va., 14–23 (1964)

Williams, J. C., Kelly, G. B., and Best, R. L.Method of Deacidifying Paper. U.S. Patent 3,898,356 (1975).

Mouradgea d'Ohsson, Ignatius. Tableau général de l'Empire othoman, divisé en deux parties, dont l'une comprend la legislation mahometane. Paris: Imprimerie De Monsieur (Firmin Didot) Vol. 2 (1788–1824).

Tang, L. C.Journal of the American Institute for Conservation. Vol. 17, No. 2, p. 19 (1978).

Kelly, G. B.Archives Et Bibliotheques De Belgique. No. 12, p. 91–105 (1974).

Barrow, W. J. “A Two Year Research Program,” Permanence/Durability of the Book. Richmond, Va., p. 21–22 (1964).

Browning, B. L. and Wink, W. A.TAPPI, Vol. 51, No. 4, 156–163 (1968).

Sampson, R. L.American Laboratory. p. 81–84 (1977).

Czepiel, T. P.TAPPI, Vol. 43, No. 4, p. 289–299 (1960).

Spinner, I. H., Mackinnon, M. H., and Lilley, J. W.Pulp and Paper Magazine of Canada, T144–T118 (1966).


Copyright © 1979 American Institute of Historic and Artistic Works