JAIC 1982, Volume 21, Number 2, Article 2 (pp. 35 to 42)
JAIC online
Journal of the American Institute for Conservation
JAIC 1982, Volume 21, Number 2, Article 2 (pp. 35 to 42)

RESTORATION OF A LARGE CHINESE BRONZE URN

Aron A. Apisdorf



7 NEARLY THREE YEARS LATER

At this time, the urn was inspected. Under very close observation, no deterioration is in evidence and the urn's condition has not altered in any way (Fig. 6).


Copyright 1982 American Institute of Historic and Artistic Works