JAIC 1983, Volume 23, Number 1, Article 5 (pp. 47 to 62)
JAIC online
Journal of the American Institute for Conservation
JAIC 1983, Volume 23, Number 1, Article 5 (pp. 47 to 62)

THE BLISTERING OF PAPER DURING HYDROGEN PEROXIDE BLEACHING

Daniel Clement


ABSTRACT—An experiment is described which relates the amount of damage to certain degraded papers caused by the formation of gas-incurred delaminations during aqueous hydrogen peroxide bleaching to variations in treatment conditions. While some treatment modifications decreased the severity of the blistering, none prevented the problem entirely.

Article Sections:

1. INTRODUCTION
2. EXPERIMENTAL PROCEDURE
3. RESULTS
4. CONCLUSIONS
5. SUMMARY
a: References
Entire Article

Copyright © 1983 American Institute of Historic and Artistic Works