JAIC 1984, Volume 24, Number 1, Article 6 (pp. 53 to 56)
JAIC online
Journal of the American Institute for Conservation
JAIC 1984, Volume 24, Number 1, Article 6 (pp. 53 to 56)

NOTES ON A METHOD FOR CONSOLIDATING LEATHER

Morgan W. Phillips


ABSTRACT—An experimental method of consolidating leather by the precipitation within the leather of polymethyl acrylate is described.

Article Sections:

1. AN ACRYLIC PRECIPITATION METHOD
2. TEST APPLICATIONS
3. FURTHER CONSIDERATIONS
4. CONCLUSION
a: References
Entire Article

Copyright 1984 American Institute of Historic and Artistic Works