JAIC 1986, Volume 25, Number 1, Article 4 (pp. 39 to 48)
JAIC online
Journal of the American Institute for Conservation
JAIC 1986, Volume 25, Number 1, Article 4 (pp. 39 to 48)

GENERAL EFFECTS OF AGEING ON TEXTILES

Randall R. Bresee




REFERENCES

Struik, L.C.E. “Physical Ageing in Amorphous Polymers and Other Materials.” New York: Elsevier, 1978.

Sung, C.S.P.; Lamarre, L.; Chung, K.H. “Use of Azochromophoric Labels as a Molecular Probe of Physical Ageing in Amorphous Polymers.” Macromolecules14 (1981): 1839.

Phillips, D.G. “Detecting a Glass Transition in Wool by Differential Scanning Calorimetry.” Textile Research Journal, 55 (1985): 171.

Brandup, J; Immergut, E.J. “Polymer Handbook.” 2nd Ed.New York: Wiley-Interscience, 1975.

Fuzek, J.K. in “Water in Polymers.” ACS Symposium Series. No. 127 (1980) Washington, D.C.: American Chemical Society.

Bresee, R.R.; Chandrashekar, V.; Jones, B.W. “Age Determination of Textiles from Single-Fiber Creep Measurements.” in Advances in Chemistry Series No. 212 (1986), Conservation and Characterization of Historical Textile and Paper Materials, Needles, H.L. and Zeronian, S.H., eds.Washington, D.C.: American Chemical Society.

Bresee, R.R.; Goodyear, G.E. “Fractography of Historic Silk Fibers,” in Advances in Chemistry Series No. 212 (1986), Conservation and Characterization of Historical Textile and Paper Materials, Needles, H.L. and Zeronian, S.H, eds.Washington, D.C.: American Chemical Society.

See for example, Labana, S.S. “Ultraviolet Light Induced Reactions in Polymers.” Washington, D.C.: American Chemical Society, 1976.

Bowmer, T.N.: Cowen, L.K.; Nichol, J.M.; O'Donnell, J.H.; Rahman, N.P.; Smith, C.A.; Winzor, D.J.; “Determination of Scission and Crosslinking Yields in Irradiated Polymers: Molecular Weight Distribution Effects for Soluble Polymers.” Polymer Preprints20(1) (1979): 376.

Clough, R.L.; Gillen, K.T.; “Techniques for Studying Heterogeneous Degradation in Polymers.” Polymer Preprints25 (1) (1984) 83.

Gvozdic, N; Dole, M. “Crosslinking and Crystallinity in Irradiated Polyethylene.” Polymer Preprints19(1) (1978) 584.

Carlsson, D.J.; Wiles, D.M. “Effects of UV Light on the Chemical and Mechanical Properties of Fiber Forming Polymers.” in “Ultraviolet Light Induced Reactions in Polymers,” Labana, S.S., ed.Washington, D.C.: American Chemical Society, 1976.

Morgan, R.J.; Pruneda, C.O.; Kong, F-M.; “Ageing Studies of Kevlar 49 Fibers.” Polymer Preprints25(1) (1984) 189.

See for example, Hawkins, W.L., ed. “Polymer Stabilization.” New York: Wiley Interscience, 1972.

Madorsky, S.L. “Thermal Degradation of Organic Polymers.” New York: Wiley Interscience, 1964.

Chemical and Engineering News, March 26, 1984, 27.

Van Krevelen, D.W. “Properties of Polymers: Their Estimation and Correlation with Chemical Structure.” 2nd editionNew York: Elsevier, 1976.


Copyright 1986 American Institute for Conservation of Historic and Artistic Works