NOTE ON A FILL MATERIAL FOR WATER SENSITIVE OBJECTS

PAMELA HATCHFIELD


ABSTRACT—The use of glass microspheres in Acryloid B-72 is discussed as a gap filler for water sensitive materials. The reconstruction of a polychromed wood Egyptian shawabti using these materials is described.